Color masterbatch injection caused problems and their solutions | |
Release time£º2016/9/24 | |
1, gloss is not good reason: nozzle outside temperature is low, the molding cycle is long, masterbatch used in titanium pigment, pigment dispersion in the masterbatch. Solution: increase the nozzle temperature, shorten the molding cycle. Reduce the titanium pigment color masterbatch, improve pigment dispersion in the masterbatch. Two causes: uneven, colour and lustre of material cylinder temperature is high, the molding cycle is long and resin compatibility is bad. Solution: to lower the cylinder temperature, USES the carrier with good compatibility.
|
|